Concrete production ; calcium-silicon ratio of concrete raw material (w(Ca) /w(Si))=0.56; autoclaved aerated ; copper tailings

Categories:
Categories:
Unit processes/Materials production/Other mineralic materials
Location:
JX-CN
Reference year: 2021 -
Description

Copper tailings replace sand in autoclaved aerated concrete production When using this life cycle inventory (LCI) data, it is critical to only include it for AAC production where copper tailings are substituted for sand and a portion of cement. The appropriate calcium-silicate ratio (w(Ca)/w(Si)) of 0.56 should be maintained. Note that the system boundary excludes the transportation of other raw materials outside the factory and does not account for the potential environmental impacts after the production of the copper tailings AAC product. Actual production data and on-site research from companies in Jiangxi Province in 2019 should be referenced for accurate assessments.

Technology

Casting molding - dry heat static stop - cutting - autoclave maintenance

Process type
Fully aggregated
LCI modeling approach
Unknown
Multifunctional modeling
NONE
Format
ILCD
Aggregation type
VERTICAL
Data provider
TianGong
Review status
Internal
Cost
Free
Contact
Tiangong LCI Data Working Group